Reactive magnetron sputtering as a tool for tailoring the electrochemical properties of thin iridium oxide electrocatalysts for water electrolysis

article
2027
authors
Koch, A. and Morales-Santelices, J. and Wünsch, F. and Walter, D.
journal
Electrochimica Acta

abstract

Reducing iridium usage is a prerequisite for lowering the capital costs of proton exchange membrane water electrolyzers (PEMWEs) and enabling large-scale deployment. In this context, reactive magnetron sputtering provides a time-efficient and solvent-free route for fabricating ultrathin Ir-based catalyst layers. In this study, we fabricate 50-nm-thick IrOx thin films with varying oxygen content directly via reactive magnetron sputtering using a pure iridium target and oxygen as a reactive gas. Using Raman spectroscopy, we show that depending on the exact sputtering process, customized layers can be fabricated containing various mixtures of iridium oxide in Ir3+ and Ir4+/Ir4.X+ configuration. In our study, we find samples with lower oxygen content, featuring a mole fraction between 21 %a (IrOx-low) and 37 %a (IrOx-middle), showing a significant share of Ir3+, while samples with a high oxygen content of 64 %a (IrOx-high) are strongly dominated by Ir4+/Ir4.X+ configuration. Electrochemical analysis in a rotating disk electrode setup under acidic conditions reveals, that layers featuring higher concentrations of Ir3+ kinetically favor the oxygen evolution reaction, but suffer from reduced stability. In contrast, layers with higher concentrations of Ir4+/Ir4.X+ are less active in comparison but more stable. The extracted Tafel slopes range between 47 mV dec1 for IrOx-high layers and 38 mV dec1 for IrOx-middle layers and are slightly lower than observed for pure Ir films. Within our electrochemical analysis, we additionally investigate the influence of catalyst conditioning by cyclic voltammetry. Interestingly, in contrast to the samples with low oxygen content, the samples with the highest oxygen content are not susceptible to the conditioning process, suggesting that no further oxidation of the layer occurs. Additionally, no changes in material composition or morphological alterations are observed in these samples. In contrast, all other samples feature strong morphological alterations upon electrochemical stressing.