UV stable passivation stack with plasma-enhanced atomic layer deposition of aluminum oxide from an industrial tube-type direct PECVD system

misc
23.09.2025
authors
Min, B.
featured_in
42nd European Photovoltaic Solar Energy Conference and Exhibition (EU PVSEC), Bilbao, Spain